Coal Grinding - Cement Plant Optimization
Drying of moisture in coal is achieved normally by ducting part of the kiln exhaust gas through the mill with inlet temperatures of up to 300°C. Inert kiln exhaust gases with oxygen content of about 3-5% are most suitable for the intended purpose due to high risk of fire/explosion in fine coal.