PFEIFFER PRODUCTS FOR THE GYPSUM INDUSTRY
5 //Heating natural gypsum or gypsum mixes in the MPS mill only until their surface moisture is fully evaporated is called grinding-drying. To do this, the mill is operated at a gas temperature of max. 90 °C after classifier. During grinding-drying the product temperature is approximately 80-85 °C, no calcining occurs and the dihydrate content